Polymeric materials, which are currently very often used in various industries, are often transported and stored in the form of granules before processing. This method has several advantages, but in most studies the test samples are modified to different shapes and dimensions. This paper is therefore focused on the initiation of selected granular plastics. Samples of five polymeric materials were exposed to an external heat flux from 20 kW.m−2 to 40 kW.m−2. A spark initiator was used to ignite the released gaseous products of thermal decomposition of the polymer sample. FTP (flow-time product) method was applied to the obtained parameter - time to ignition, from which other initiation parameters were determined. The critical heat flux was determined in the range of 5.0 kW.m−2 - 11.8 kW.m−2. Despite the relatively small thickness (4 mm), the samples behaved as thermally thick. During the measurement, thin surface layer melted, and the rest of the polymer remained in its original granulated form. Ignition temperatures were calculated according to the Stefan-Boltzmann’s law between 273 °C - 402 °C.
Reference25 articles.
1. [1] GEYER, R., JAMBECK, J. R., LAW, K. L. 2017. Production, use, and fate of all plastics ever made. Supplementary materials. Science advances, 3(7), e1700782. ISSN 2375-2548.
2. [2] PLASTICS EUROPE. 2018. Plastics – the facts 2018, An analysis of European plastics production, demand and waste data. 60.
3. [3] JANG, B. N., JUNG, I., CHOI, J. 2009. Study of a novel halogen-free flame retardant system through TGA and structure analysis of polymers. Journal of applied polymer science, 112(5), 669-2675. ISSN 1097-4628.
4. [4] PIELICHOWSKI, K., NJUGUNA, J. 2008. Thermal degradation of polymeric materials. 1st ed. iSmithers Rapra Publishing, 2008. 316 p. ISBN 1-85957-498-X.
5. [5] PETERSON, J. D., VYAZOVKIN, S., WIGHT, C. A. 2001. Kinetics of the thermal and thermo-oxidative degradation of polystyrene, polyethylene and poly (propylene). Macromolecular Chemistry and Physics, 202(6), 775-784. ISSN 1521-3935.
Cited by
1 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献