Slow Growth Damage Assessment of Bonded Metal-Composite Joint Using a Numerical Approach

Author:

Kabir Md. Imran12,Wong Laurence1,Wang John3,Yang Chunhui1,Zhang Y. X.1ORCID

Affiliation:

1. School of Engineering, Design and Built Environment, Western Sydney University, NSW 2751, Australia

2. Department of Civil and Environmental Engineering, Islamic University of Technology, Gazipur 1704, Bangladesh

3. Aerospace Division, Defence Science and Technology (DST) Group, Melbourne, Australia

Abstract

The applications of composite materials and adhesive-bonded joints in the aviation industry have significantly increased in recent years and their damage assessment attracts a lot of research interest. This study investigates the slow growth damages of bonded metal-composite joints and develops a finite element-based numerical procedure to capture mechanical behaviors of those damages in the joints. The residual static strength and strain energy release rates (SERRs) (which determine the damage growth rates) of the joints are the two quantities that can be determined to predict the fatigue life of adhesive bonded joints. The absence of extensive experimental and numerical assessments for predicting the slow growth damage of bonded metal-composite joints necessitates the development of a numerical procedure to determine these quantities. Toward this end, a three-dimensional (3D) finite element (FE) model was created. From the FE analyses, the residual static strength and SERRs of bonded metal-composite joints were calculated as a function of varying disbond crack lengths following the adhesive element failure criterion and fracture mechanics approach, respectively. Additionally, the residual strength and SERR for joints with delamination of the composite adherend were also calculated by implementing a linear fracture mechanics-based failure index. The results suggested that the stable crack length of the joint with 180[Formula: see text]mm long overlap length was about 140[Formula: see text]mm and 100[Formula: see text]mm when the crack was initiated from taper and gap end, respectively. These lengths were consistent for both disbond and delamination scenarios. Residual strength values were 89[Formula: see text]kN and 65[Formula: see text]kN for joints with 10[Formula: see text]mm disbonds initiated from the taper end and gap region, respectively. With the material properties considered, the delamination propagation strengths for delaminated joints were notably lower than their disbonded counterparts. Based on the findings of this study’s analysis, a systematic strategy was developed for applying the slow growth technique for bonded joints, which would aid in the creation of an actual sample for experimental validation. The experiment in turn will provide calibration for the parameters in the model for practical applications.

Funder

Department of Defence, Australian Government

Publisher

World Scientific Pub Co Pte Ltd

Subject

Mechanical Engineering,Mechanics of Materials,General Materials Science

Cited by 2 articles. 订阅此论文施引文献 订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3