Optimizing the sintering process parameters for simultaneous improvement of the compression strength, impact strength, hardness and corrosion resistance of W–Cu nanocomposite

Author:

Samadi Mohammad Reza1ORCID,Zeynali Ebrahim2,Allahyari Fatemeh3,Salahshorrad Ehsan4ORCID,Zangeneh-Madar Karim4,Afshari Mahmoud5ORCID

Affiliation:

1. Faculty of Mechanical Engineering, Technical and Vocational University (TVU), Tehran, Iran

2. Department of Mechanical Engineering, Iran University of Science and Technology (IUST), Tehran, Iran

3. Faculty of Sciences, Arak University, Arak, Iran

4. Faculty of Materials and Manufacturing Technologies, Malek Ashtar University of Technology, Tehran, Iran

5. Department of Mechanical Engineering, Amirkabir University of Technology, Tehran, Iran

Abstract

The main purpose of this work is to optimize the mechanical properties of tungsten–copper (W–Cu) nanocomposite fabricated by the sintering process. For this purpose, the parameters of sintering temperature, sintering time and weight percentage of copper were selected to optimize the compression strength, impact strength, hardness and corrosion resistance of the W–Cu nanocomposite using the desirability function procedure and response surface method. The analyses of transmission electron microscopy (TEM), scanning electron microscopy (SEM), energy dispersive X-ray spectroscopy (EDS) and X-ray diffraction (XRD) were also performed to examine the microstructure of W–Cu nanocomposite. The results exhibited that a rise in the sintering temperature from 1000C to 1150C significantly enhanced the impact strength of W–Cu nanocomposite, while a rise in the sintering temperature from 1150C to 1300C deteriorated the impact strength. Moreover, the compression strength and hardness of the W–Cu nanocomposite continuously improved by elevation of sintering temperature from 1000C to 1300C. A rise in the amount of Cu from 20[Formula: see text]wt.% to 40[Formula: see text]wt.% led to a reduction in the hardness of the W–Cu nanocomposite, while a rise of Cu content improved the impact and compression strengths. The results also indicated that the mechanical properties of W–Cu nanocomposite enhanced simultaneously by using 27[Formula: see text]wt.% Cu at sintering temperature of 1197C and sintering time of 2.7[Formula: see text]h. The samples sintered at the optimal conditions indicated a higher corrosion resistance than that sintered at the initial conditions.

Publisher

World Scientific Pub Co Pte Ltd

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3