Abstract
This study evaluated the shear bond strength of porcelain/composite using 40 metal + porcelain + composite cylindrical specimens divided into 4 groups, according to porcelain surface treatment: 1) no treatment, 2) mechanical retentions performed with diamond burs, 3) etching with phosphoric acid+silane, and 4) etching with hydrofluoric acid+silane. After being stored in distilled water at room temperature for one week, the specimens were submitted to a shear force (load) and the data were analyzed statistically (ANOVA). The means (in Mpa) of the groups were: 4.71 (group 1); 4.81 (group 2); 11.76 (group 3); 11.07 (group 4). There were no statistically significant differences between groups 1 and 2 and between groups 3 and 4.
Reference20 articles.
1. Repairing porcelain restorations intraorally: techniques and materials;Zhukovsky L;Comp Cont Educ Dent,1996
2. Repairing fractured porcelain: how surface preparation affects shear force resistance;Pameijer CH;J Am Dent Assoc,1996
3. Bonding strengths of porcelain repair systems with various surface treatments;Chung KH;J Prosthet Dent,1997
4. Comparison of composite resin-to-porcelain bond strength with three adhesives;Kelsey WP;Gen Dent,2000
5. Clinical study on the reasons for and location of failures of metal-ceramic restorations and survival of repairs;Özcan M;Int J Prosth,2002
Cited by
30 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献