The Effect of Solution Treatment Duration on the Microstructural and Mechanical Properties of a Cold-Deformed-by-Rolling Ti-Nb-Zr-Ta-Sn-Fe Alloy
-
Published:2024-02-13
Issue:4
Volume:17
Page:864
-
ISSN:1996-1944
-
Container-title:Materials
-
language:en
-
Short-container-title:Materials
Author:
Cojocaru Vasile Dănuț1ORCID, Șerban Nicolae1ORCID, Cojocaru Elisabeta Mirela1, Zărnescu-Ivan Nicoleta1ORCID, Gălbinașu Bogdan Mihai2ORCID
Affiliation:
1. Faculty of Materials Science and Engineering, National University of Science and Technology Politehnica of Bucharest, 060042 Bucharest, Romania 2. Dental Medicine Faculty, University of Medicine and Pharmacy “Carol Davila” Bucharest, 020021 Bucharest, Romania
Abstract
The study presented in this paper is focused on the effect of varying the solution treatment duration on both the microstructural and mechanical properties of a cold-deformed by rolling Ti-30Nb-12Zr-5Ta-2Sn-1.25Fe (wt.%) alloy, referred to as TNZTSF. Cold-crucible induction using the levitation synthesis technique, conducted under an argon-controlled atmosphere, was employed to fabricate the TNZTSF alloy. After synthesis, the alloy underwent cold deformation by rolling, reaching a total deformation degree (total applied thickness reduction) of 60%. Subsequently, a solution treatment was conducted at 850 °C, with varying treatment durations ranging from 2 to 30 min in 2 min increments. X-ray diffraction (XRD) and scanning electron microscopy (SEM) techniques were utilized for the structural analysis, while the mechanical properties were assessed using both tensile and hardness testing. The findings indicate that (i) in both the cold-deformed-by-rolling and solution-treated states, the TNZTSF alloy exhibits a microstructure consisting of a single β-Ti phase; (ii) in the solution-treated state, the microstructure reveals a rise in the average grain size and a decline in the internal average microstrain as the duration of the solution treatment increases; and (iii) owing to the β-phase stability, a favorable mix of elevated strength and considerable ductility properties can be achieved.
Reference60 articles.
1. Katti, K.S., Verma, D., and Katti, D.R. (2008). Joint Replacement Technology, Woodhead Publishing. 2. Goharian, A., and Abdullah, M.R. (2017). Bioinert Metals (Stainless Steel, Titanium, Cobalt Chromium). Trauma Plat. Syst., 115–142. 3. Prasad, K., Bazaka, O., Chua, M., Rochford, M., Fedrick, L., Spoor, J., Symes, R., Tieppo, M., Collins, C., and Cao, A. (2017). Metallic Biomaterials: Current Challenges and Opportunities. Materials, 10. 4. Intraosseous metal implants in orthopedics: A review;Rony;Morphologie,2018 5. Biocompatible Titanium Alloys used in Medical Applications;Baltatu;Rev. Chim.,2019
|
|