Abstract
The water corrosion of tungsten as a target material can affect the safe operation of accelerator-driven neutron source. This paper reported the corrosion behaviors of tungsten in ultrapure water and tap water for 7, 14, 21, 30 and 60 days. Moreover, ICP-MS, XRD, XPS, SEM-EDS and LSCM were used to analyze the components in solutions, crystalline structures, chemical compositions and surface morphologies. It was found that the dissolution of tungsten, due to corrosion, reached its maximum between 30 days and 60 days in both solutions. The cube-shape substance, CaWO4, was the main corrosion product after tungsten in tap water. The tungsten oxide was changed from WO3 to WO2 during the corrosion of tungsten in ultrapure water. Compared with tungsten in ultrapure water, tungsten in tap water had its surface completely destroyed, with a dense diamond shape. Therefore, based on the analysis from this study, the corrosion mechanisms of tungsten in ultrapure and tap water were revealed.
Funder
Guangdong Basic and Applied Basic Research Foundation
Subject
General Materials Science
Cited by
1 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献