Stress Relaxation of Natural and Synthetic Rubber Stocks

Author:

Tobolsky A. V.1,Prettyman I. B.1,Dillon J. H.1

Affiliation:

1. 1The Firestone Tire & Rubber Company, Akron, Ohio

Abstract

Abstract 1. The complete decay of stress in the rubbers studied, held at constant elongation, appeared to involve the rupturing of a definite bond, either at some point along the molecular chain or at the cross-linking bond put in by vulcanization. In the case of a Hevea rubber gum stock the data could be fitted very well by ordinary reaction-rate theory, leading to the conclusion that the free energy of activation required for breaking the bond is 30.4 kcal. per mole of bonds. This result was found to be practically independent of the elongation, and of the presence of carbon black in a Hevea rubber tread stock. This is to be compared to a strength of about 90 kcal. per mole for the C—C bond. 2. In the case of other rubbers (Buna-S, Butaprene-N, Neoprene-GN, and Butyl) the activation free energy for breaking the bond did not vary by more than ±2.0 kcal. per mole from that of Hevea rubber. However, these differences were quite definite. For example, the relaxation of stress in GR-S was slower than in Hevea; a small difference in energy corresponding to a 2:1 ratio in the respective times of decay. 3. The effect of temperature on the relaxation of stress appeared to be of the general type characteristic of chemical reactions. By use of the ordinary formula for expressing rate of reaction in terms of energy of activation, one could predict very closely the behavior of the stress-log time curves at different temperatures. 4. Natural rubber and GR-S vulcanized with paraquinone dioxime and lead dioxide showed relaxation curves very similar to those of the sulfur vulcanized stocks. 5. Relaxation experiments in an ordinary air atmosphere and in an atmosphere of commercial nitrogen showed no appreciable differences. 6. Examination of stretched rubber bands in which the stress had decayed nearly completely (at 100° C) gave no evidences of gross oxidation, such as would make the rubber bands sticky or hard, or of surface deterioration. At higher temperatures, however, the rubber could be observed getting sticky, and then brittle. Specimens in which the stress had completely decayed showed very low tensile strength (by hand test). 7. Antioxidant added to a sulfur-stabilized Buna-S stock caused a definite retardation of the rate of relaxation. 8. Comparison of the results of these experiments with previously recorded observations in the literature indicated that the chemical reaction which ruptured the rubber structure and caused the decay of stress in these experiments (and concomitantly a lowering of tensile strength) was an oxidation of the rubber by small amounts of oxygen, the reaction rate being independent of the oxygen pressure in the range between that present in an ordinary air atmosphere and in a commercial nitrogen atmosphere. 9. The tests suggested a convenient and accurate laboratory method of determining the oxidizability of natural and synthetic rubber stock designed for service.

Publisher

Rubber Division, ACS

Subject

Materials Chemistry,Polymers and Plastics

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3