Author:
Oh Jung-Min,Yang Jaeyeol,Yoon Jaesik,Lim Jae-Won
Abstract
In this study, an effective method is demonstrated for fabricating titanium sputtering targets, which are used to fabricate thin films in the semiconductor industry. The method is an alternative to the existing electron beam melting (EBM) process under high vacuum. Titanium sputtering targets used in the production of semiconductors must have very low concentrations of gaseous impurities, especially oxygen, as well as metal impurities. Currently, the oxygen concentration in titanium sputtering targets used for industrial purposes is less than 400 ppm. To develop an effective alternative method, powder metallurgy and melting processes were performed to prepare a low-oxygen titanium ingot with less than 400 ppm oxygen. First, titanium powder was deoxidized using calcium vapor, and then the powder was subjected to vacuum arc melting (VAM). The oxygen in the titanium powder was reduced with calcium vapor from an initial concentration of 2200 ppm to 800 ppm, and the resulting powder was melted using VAM, resulting in titanium ingots with low oxygen content, 400 ppm or less. It was also confirmed that all lattice constants, i.e., <i>d, a, c,</i> and <i>c/a</i>, decreased as oxygen concentration decreased in both the titanium powder and the ingots.
Funder
Korea Institute of Energy Technology Evaluation and Planning
Ministry of Trade, Industry and Energy
National Research Foundation of Korea
Ministry of Education
Publisher
The Korean Institute of Metals and Materials
Subject
Metals and Alloys,Surfaces, Coatings and Films,Modelling and Simulation,Electronic, Optical and Magnetic Materials
Cited by
6 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献