AbstractCross-laminated timber (CLT) panels – consisting of several cross-wise stacked layers of glued boards – have a high dimensional stability. However, the outer surfaces of CTL are exposed to environmental humidity changes and thus to swelling and shrinking. To improve CLT’s dimensional stability further, the layers of kiln dried (KD) CLT were substituted partly (on the surfaces) and entirely with superheated steam treated (SHST) wood. The effects of SHST wood and the performance of the one-component polyurethane resin (PUR) were tested by block shear and delamination tests after water soaking. Under various conditions, the shear strength ranged from 1.3 MPa to 4.7 MPa and the wood failure percentage (WFP) from 76% to 92%. The optimal parameter were ascertained as pressing time (30–45 min), pressure (0.98 MPa) and adhesive amount (175–200 g m−2). The water soaked delamination of CLT manufactured with SHST wood was approximately 50% lower than that of CLT made of KD wood.
Cited by
8 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献