Publisher
Springer Nature Singapore
Reference40 articles.
1. Tran NP, Gunasekara C, Law DW, et al. A critical review on drying shrinkage mitigation strategies in cement-based materials. J Build Eng. 2020;2021(38): 102210.
2. Wu Z, Shi CJ, Khayat KH. Multi-scale investigation of microstructure, fiber pullout behavior, and mechanical properties of ultra-high performance concrete with nano-CaCO3 particles. Cement Concr Compos. 2018;86:255–65.
3. Yoo DY, Banthia N, Yoon YS. Ultra-high-performance fiber-reinforced concrete: Shrinkage strain development at early ages and potential for cracking. J Test Eval. 2017;45(6):2061–70.
4. Wang L, Zhou SH, Shi Y, et al. Effect of silica fume and PVA fiber on the abrasion resistance and volume stability of concrete. Compos B Eng. 2017;130:28–37.
5. Sanchayan S, Foster SJ. High temperature behaviour of hybrid steel–PVA fibre reinforced reactive powder concrete. Mater Struct. 2016;49(3):769–82.